HJ260, Fused Welding Fluxes Applied to HOCr21Ni10,HOCr20Ni1OTi,H1Cr13,H3Cr13,etc
  • HJ260, Fused Welding Fluxes Applied to HOCr21Ni10,HOCr20Ni1OTi,H1Cr13,H3Cr13,etc
  • HJ260, Fused Welding Fluxes Applied to HOCr21Ni10,HOCr20Ni1OTi,H1Cr13,H3Cr13,etc

HJ260, Fused Welding Fluxes Applied to HOCr21Ni10,HOCr20Ni1OTi,H1Cr13,H3Cr13,etcBT003519

Brand:
$0.00 USD

Note: Different prices will be automatically shown above when you input different level quantity for each relevant specification. Once your quantity lies in “inquiry”, please add it to cart and continue shopping, we will confirm you the price shortly once you submit the order successfully.

Units Price per Unit (1 Unit = 1 Ton)
0Need to log in
1--5Need to log in
6--10Need to log in
above11Need to log in

This item has been added to shopping cart.

View Shopping Cart  Continue Shopping

Groupbuy Wishlist

Lower Price, Buy Together. We will release the groupbuy for this item by collecting the information from your Groupbuy Wishlist and offer you an unbelievable price.

*

*

*

 

                                                                       

Description

HJ260 is a kind of smelting-type low-Mn high-Si and mid-F flux.it appears grey glassy particles with the mesh of 10-60(2-0.3mm).During the course of welding,direct-current main is adopted and welding wires are connected to the positive electrode. It has the advantages in application of stable arc,fine appearance of bead and fine detachability.


Usage&Cautions

● It can be used in the welding of relevant acid-proof stainless struc-tures in conjunction with austenitic stainless welding wires (such as HOCr21Ni10,HOCr20Ni1OTi,H1Cr13,H3Cr13,etc).It is also used in the submerge-arc build-up welding of all kinds of continuous cast rollers,hot-rolled rollers,mid-or small-sized steel rollers,corrosion-proof shafts,wheels,etc with excellent performance.

● Impurities on the welding surface must be removed before welding,such as oil soil,moisture,iron rust,etc.
● The flux must be baked for 2 hours under the temperature of 300-400℃ before it is used.

 

Specification

(Chemical Composition)(%)

 SiO2  CaF2  Al2O3+MnO  CaO+MgO  FeO  S  P
 29~34  20~25  20~28  20~25  ≤1.0  ≤0.06  ≤0.07

 

Mechanical Performance

 Item  Yield pointбb(MPa)  Tensile Strength бb(MPa)  Elongation δ5(%)
 Standard   ≥400   ≥550   ≥35%

 

Packing details

 Pallet  22tons/pallet
 Bag  25kg/bag

 

Note: The price base on 1unit=1ton

 

There are currently no optional accessories for this item.